Hi,

I've been etching Ti3AlC2 MAX phase in the lab for a year, having made several batches. In the last 3 I've been observing a peak at around 44°. This peak is observed for multilayer and delaminated samples.

Is this contamination of undissolved LiF crystals ?

If so, to mitigate this should I use more washing cycles ?

The substrate I use for analysing the samples is Si (100).

Thank you