I have a query is that after crystallization peak point some of other noise type peaks occur in DSC scan for (Se78-xTe20Sn2Znx) x=2 and x=6 ,this peak shown the material property or due to atmospheric condition. Please explain me.
and I have another question about the DSC peak. Can you please explain me, is glass transition peak represents the material's rigidity or it signifies something else?