I am preparing cellulose nanocrystals by acid hydrolysis. After centrifugation step, I put the dispersion in dialysis bag until constant pH. In order to use shorter length of dialysis bag (they are rather expensive), I use high concentrations (more than 5 wt%) and after 9 days I reach to nearly pH 7.  But in some papers, it is recommended to use very dilute concentrations of CNC.

Does the concentration only affect the time to reach neutral pH or something else?