I am in confusion about - in chemical bath deposition if precursor concentration increaed the thickness of film decreased.
can anybody explain this or provide reference pl.
You should check the ammonia concentration (agent complexing) used in CBD technique
What this unit identifies for the ion exchange capacity ca. 0.92 meq. g-1. I am a newcomer in the membrane area. I just started. I highly appreciate your help
08 May 2021 0 0 View
We use reactive sputtering process to make aluminum nitride film, and want to make c-axis aluminum nitride film on a silicon substrate, but the crystal orientation cannot be seen with...
03 March 2021 7,975 3 View
Anyone can recommend any books on such topics? Thanks in advance.
02 March 2021 8,457 2 View
(This statement is from wikipedia, BTW). What is so special about metallic bond that is limiting high-P low-T state of a matter (as long as individual atoms exist, not white dwarf of neutron star...
02 March 2021 3,309 2 View
The Lanthanide contraction which is the decrease in ionic radii of the elements in the lanthanide series from atomic number 57, lanthanum, to 71, lutetium, is due to poor shielding of the 4f...
01 March 2021 2,272 4 View
Hi all, I need to cleave the ester in Ethyl 2-amino-1H-imidazole-5-carboxylate to make the carboxylic acid and retrieve the product from solution to use in downstream applications of linking to...
01 March 2021 8,766 3 View
I am a little confuse with the mechanism of solid lipid nanoparticles (SLNs). The main point of encapsulating drugs into SLNs is because some drugs have low solubility in water. Therefore, SLNs...
01 March 2021 3,703 3 View
I try to check the uv-vis absorption of Indium nanoparticle. Now I am measuring in solution, can I measure it in the form of a film?
01 March 2021 930 3 View
Favourable conditions of base pressure, rate of deposition. Also, by which characterisation technique to be used to verify the thickness of the deposited film.
28 February 2021 3,640 3 View