Hello guys,
I am optimizing a perovskite photodetector device with the device structure ITO/PTAA/Cs0.15FA0.85PbI3/PCBM/BCP/Ag.
PTAA (2 mg/mL): 5000 rpm/30 sec
Perovskite (1.3 M): 1000 rpm/10 sec. and 5000 rpm/30 sec. In the last 10 seconds, EA (ethyl acetate) was used as the antisolvent to increase crystnillity.
PCBM (20 mg/mL): 2000 rpm/30 sec
BCP (0.5 mg/mL): 5000 rpm/30 sec
Till now, I can achieve Jsc around 16 mA cm^-2.
Please, anyone suggest how to make it above 20 mA cm^-2?