I have prepared a 1-gallon alumina polishing slurry with the following formulation:

-Alumina (2.5 microns, 20.5%)

-DI water (70.3(%)

-Dispersant (4%)

-PVA 205 as a binder (2%)

-Aluminum nitrate nonahydrate as an accelerator (3%)

-Defoamer (0.2%).

To create the slurry, I stirred the alumina, DI water, and dispersant for 5 hours at 500 RPM. The other additives were then added at different time intervals. After the preparation, the PH and viscosity were within acceptable ranges. However, when used for polishing, the slurry tends to form a haze on the glass surface. Could someone please provide guidance on how to address this matter?