who can help me for microetchant of Haynes 188 (Co-22Ni-22Cr-14W-3Fe-0.1C)? please guide me with detail...Thank you.
we want reducing Carbon content of initial electrode of VAR furnace, electrode composition prepared for VAR is (FSX-414: 52Co 29Cr 10Ni 7W) but Carbon is higher than limited composition (about...
11 December 2019 7,423 3 View
we want to produce VAR electrode (d=150 mm) from scraps (Ti 6-4) for melting (with attached shape). what is best solution for producing of initial electrode? can we cut it to small pieces and...
10 November 2019 9,378 2 View
who can help me about "Incoloy 907" its (Fe-Ni-Co-Nb-Ti) superalloy. i need some information about: product approach, deformation, heat treatment and microstructrue. please guide me.
06 July 2017 9,797 6 View
hello after hot rolling with 2 different reduction of thickness (60% and 85%) on haynes 188 (Carbide strengthened and solid solution Cobalt base alloy) we observed sample with 85% reduction of...
04 May 2017 1,507 6 View
hi everyone, we conducted hot tension test on Haynes 188 (Co base superalloy) at 1100 C, 1150 C, 1175 C and 1200 C. but magnitude of ductility decrease after 1150 C. we evaluate microstructure...
31 December 2016 2,289 7 View
what is best etchant for revealing microstructure of Haynes 188 (Co-base alloy)? i used below solution but result wasn't good enough. i used: 90ml HCl 37%+ 5ml H2O2 please help me. thank you all
04 May 2016 1,944 3 View
04 May 2016 5,261 1 View
i should be achieve EBSD (electron back scatter diffraction) for my current project. but we had not access to it. can i send my specimens to a corporation or institute to do it for me. please guide me
04 May 2016 3,146 5 View
look at pic. what is this precipitation and streaks? this alloy was elcroetched. 100ml water 10 ml HCl
04 May 2016 7,173 6 View
we annealing Haynes 188 (Co-base alloy) in different temperature and after we observed some twining in it (annealing twin). i want comparison whit together, i estimate volume fraction of twin...
03 April 2016 7,898 3 View
Hello everyone. Given microstructure image belongs to a 12% ledeburitic cold work tool steel (annealed and tempered). The sample was etched with picral (100 mL ethanol and 4 g picric acid). I...
02 March 2021 4,119 3 View
Which solution reveals the microstructure and features of nickel-based alloys?
02 March 2021 2,221 3 View
It is oftentimes said to be a distinctive metallographic trait that differentiates a fully austenitic and a fully felly ferritic steel without etching that might distinguish between two. Why...
02 March 2021 728 2 View
Hello everyone, I had run a mediation model in SmartPLS using questionnaires that were already validated among my statistical population. A professor who edited my paper -though she is not...
01 March 2021 3,052 3 View
I am working on modeling and simulation of biomecanical material behaviour, I have succeded on simulating skin using anisotropic hyperelastic material, on APDL and in our lab's finite element...
28 February 2021 552 3 View
Good day to all, I have no experience with light emitting diodes. I am building a glass mini flume to demonstrate the photo degradation of Methylene Blue in water running over self cleaning...
26 February 2021 4,026 5 View
I am working on TiO2 composite material and the results of XRD have a lot of small/junk peaks and while I apply a smooth filter in Origin then the other characteristics peaks disappear so anyone...
26 February 2021 8,183 3 View
For wrought alloys soaking time at solutionizing temperature is determined by thickness .Do we have such standards for cast Al alloys
23 February 2021 8,839 3 View
Hello everyone: I am looking for a simple software program to model chemical bonds. The purpose is to generate a high-quality graphical abstract for a top leading journal in the field of...
23 February 2021 8,012 3 View
I have prepared Ag-Cu alloy with polymer coating upon it.... how can I measure thermal conductivity of it ?
22 February 2021 5,915 3 View