Copper or Steel or an alloy ?!
usually Copper
Hello Farhad Moradi ,
Planchettes for TLD readers are usually made of nichrome.
Regards,
Tom Cuff
Instead of checking only the mRNA level, I want to check the active protein level of MMP-1 in Liver tissue from mice. How can I do that?
03 March 2021 1,763 2 View
I want to analyses the proportion of swimming sperm of three species of fish in two salinities. To analyse the proportion of swimming sperm in a Generalized Linear Model, I would use a Binary...
03 March 2021 2,297 3 View
03 March 2021 8,272 1 View
Hi. Please tell me what guidelines should i need to follow for questionaries' type research work in India. It is not hospital based work, we are conduction basic institutional based qualitative...
03 March 2021 2,037 3 View
Hi, I implemented a code to gabor filter cifar10 data but the images after being filtered and stacked are not clear like the original images. I think the problem is in the way I am using the...
03 March 2021 6,317 1 View
i am try to classify the x-ray images. During classification , can i block unwanted images (except x-ray image).
03 March 2021 7,100 1 View
03 March 2021 5,360 2 View
The term miscibility refers to the single-phase state in thermodynamics. I do not mean the compatibility of different components. To determine the miscibility I know several techniques such as...
03 March 2021 4,107 4 View
If the detection range is in ng/ml but the reference range is in ug/ml for a molecule or protein in serum or plasma .how to dilute and what is the initial volume to be taken for quantitative analysis
02 March 2021 7,670 3 View
02 March 2021 5,204 3 View
I looking for ferro calcium production process
03 March 2021 1,755 4 View
Hello everyone. Given microstructure image belongs to a 12% ledeburitic cold work tool steel (annealed and tempered). The sample was etched with picral (100 mL ethanol and 4 g picric acid). I...
02 March 2021 4,119 3 View
Which solution reveals the microstructure and features of nickel-based alloys?
02 March 2021 2,221 3 View
It is oftentimes said to be a distinctive metallographic trait that differentiates a fully austenitic and a fully felly ferritic steel without etching that might distinguish between two. Why...
02 March 2021 728 2 View
As I was tweaking step-by-step OpenCalphad6 Macros step1.ocm involving phase and thermal property calculation of a High-speed steel, I could not incorporate more than 6 elements in the steel...
01 March 2021 8,840 1 View
I have a structure that employs d-ring swiveling tie-downs that corrode during use and become "frozen". I have sample swivel assemblies that I wish to corrode to see if I can free them using one...
01 March 2021 3,739 3 View
I am conducting anodic electrodeposition of MnO2 onto a stainless steel substrate, using a platinum strip as a counter electrode. This is done galvanostatically, with the current held between 5...
27 February 2021 1,829 3 View
Hello everyone, I'm looking for a way to delaminate copper current collector of water-based anodes in Li-ion batteries without damaging the graphite film. I tried different materials such as HNO3...
24 February 2021 3,785 3 View
For wrought alloys soaking time at solutionizing temperature is determined by thickness .Do we have such standards for cast Al alloys
23 February 2021 8,839 3 View
My main concern is that the metal powders should not weld to the mold surface and I should easily be able to eject out the pressed samples. I am looking for alternative for graphite moulds. The...