Can help me about which is an normal requirements of decarburization in hot forging pieces?.
I have tailored my answers with materials that would guide you to see the answers you seek.
https://www.google.com/url?sa=t&rct=j&q=&esrc=s&source=web&cd=7&cad=rja&uact=8&ved=0CD0QFjAG&url=http%3A%2F%2Fwww.ijsrp.org%2Fresearch-paper-0313%2Fijsrp-p1547.pdf&ei=32OHVNSbAYSiugSIjoLQBw&usg=AFQjCNEBY4CE6cyfvdn9fN99rSsfllfbng&sig2=whLSL4wDJYzs4op85paIrA&bvm=bv.81449611,d.d24
https://www.google.com/url?sa=t&rct=j&q=&esrc=s&source=web&cd=9&cad=rja&uact=8&ved=0CEgQFjAI&url=https%3A%2F%2Fglobaljournals.org%2FGJRE_Volume12%2F5-Effect-of-Hot-Forging-on-Chemical.pdf&ei=32OHVNSbAYSiugSIjoLQBw&usg=AFQjCNFTeoNUM9MmBtVph_S7sBXu0Mk57g&sig2=-_NF6S2ErY3oX7KVDdxNqA&bvm=bv.81449611,d.d24
https://www.google.com/url?sa=t&rct=j&q=&esrc=s&source=web&cd=12&cad=rja&uact=8&ved=0CB8QFjABOAo&url=https%3A%2F%2Fwww.forging.org%2Fsystem%2Ffiles%2Ffield_document%2FFatemi1_Effect_of_forging_surface_on_fatigue_behavior_of_steels_a_literature_review.pdf&ei=NmSHVJijFY6duQTumoHYBA&usg=AFQjCNHDub_EXd_5kQIOyTxLF9n3DawWHw&sig2=ZNlWgvactBkx0xSlpZADIQ&bvm=bv.81449611,d.d24
Thanks you Sir. The information is really good.
If you have a laser cutting machine that can cut a steel sheet up to 10 mm thick, is it possible to cut a 20 mm steel sheet in two consecutive passes? If the answer is yes or no, why?
09 October 2019 9,277 3 View
I know that a way to establish the lubrication regime in a pin on disk test is by measure the resistance between the pin and the disc. Some papers say that if the resistance is of 2 ohm, the...
05 June 2019 7,779 3 View
Hi People. Here in RG there is a similar question but for works in biology. Some of you know if is there any software available to design mechanical engineering graphical abstracts ? Something...
31 December 2018 3,415 2 View
Hi People. I need to know the temperture range for making warm forging of SAE 1045 steel.
31 December 2018 4,546 0 View
Please. I need to know what level of hardness provide a equilibrated behaviour between wear resistance and toughness. Also, if a ionic nitriding treatment reduce the friction factor between the...
10 November 2018 6,466 1 View
09 October 2018 8,748 0 View
People. I need your colaboration. What value of hardness do you think is the minimal to not worsen the maquinability level of the steel? I work with steel of 0,1% C. I some of you have a paper, is...
08 September 2018 9,234 3 View
Some people say that the risk is bigger when the chip particles size are 500 micrometers or minus? What is the reason of this size?
07 August 2018 7,570 0 View
Please. I need information about the recrystallization temperature of SAE 1010 steel, and also the temperature range for warm forging.
05 June 2018 5,685 3 View
Hi People. I need your help in relation to obtain technical information about testing methodology of surgical drills used in bone applications. This information may be standards, papers, and so...
02 March 2018 2,232 6 View
I looking for ferro calcium production process
03 March 2021 1,755 4 View
Hello everyone. Given microstructure image belongs to a 12% ledeburitic cold work tool steel (annealed and tempered). The sample was etched with picral (100 mL ethanol and 4 g picric acid). I...
02 March 2021 4,119 3 View
It is oftentimes said to be a distinctive metallographic trait that differentiates a fully austenitic and a fully felly ferritic steel without etching that might distinguish between two. Why...
02 March 2021 728 2 View
Hello, I am new to biofilm research and have a question about growing and measuring biofilms. We want to research the effect of a type of enzymes in breaking down biofilms in showers, baths, hot...
14 February 2021 3,522 3 View
I want to train a model that should predict if a given signature is a genuine or a forged one. The model should take two images as input. One is the real signature, and the other is to be...
11 February 2021 4,436 3 View
Hello dear Academicians, I am working on the forging of Mo alloys, but I wanted to consult you on an issue I could not solve. Mo is easily oxidized during forging and MoO3 is formed. Is it...
09 February 2021 1,989 3 View
While CCS can be employed along with a conventional Carbon-efficient EAF steelmaking process (especially from iron ore) or even Hydrogen or hydrocarbon can bee passed through central electrode,...
30 January 2021 3,378 1 View
Basic dendrite formation of metallic alloys are explained by thermal and constitutional degree of supercooling and most-supercooled band of liquid somewhat ahead of solidification front that...
30 January 2021 8,450 2 View
To have the desired grain size in 6061 and 6063 Al alloy, what should be the minimum % of Ti and B pick up and what is the chemistry/metallurgy behind that?
07 January 2021 9,305 2 View
Here are three different ways to calculate crystallite size and lattice strain of a sample, based on XRD peaks: "Scherrer" calculation, "Williamson-Hall" or "Rietveld". Each calculation is proper...
04 January 2021 7,836 4 View