The white precipitate that remained after forming ZnO from the precursor Zinc Acetate Dihydrate was left to dry on the stove at 100 degrees Celsius overnight ( 16 hrs), and then calcinated in a muffle furnace for four hours. Is this method correct or am not going to expect the right nm size NPs.