I have deposited cds on ITO by electrodeposition. Now I want to create sharp step in film for profilometry measurement (thickness). So I want to know how to create sharp step in film either during deposition or by using suitable etchant.
what's cds? Is it CdS cadmium sulfide, or is it something else?
Yes,it is cadmium sulfide...
As-deposited CdSe films have very high resistance.What materials doping can be used to increase the conductivity?
01 February 2015 9,763 7 View
Can anyone explain in brief how to prepare the solution for ternary CdSexTe(1-x) thin films e.g. CdSe(0.6)Te(0.4) thin film?
09 October 2014 9,834 2 View
How solid solution of CdSe/PbS leads to optimum band gap?
08 September 2014 7,232 2 View
Can anyone suggest a reference electrode for electrodeposition in aqueous solution? Which one is better between a Saturated Calomel Electrode (SCE) and an Ag/AgCl reference electrode?What is the...
03 April 2014 9,788 22 View
How much feasibility of electrodeposition of SnS layer on electrodeposited ZnO nanostructures to form the ZnO/SnS heterostructure? What is the future scope of this type of heterostructures for...
03 April 2014 3,951 5 View
Ca anyone suggest some Indian manufacturers of reference electrodes e.g. SCE or Ag/Agcl for electrodeposition purpose in aqueous electrolyte. I have references of some companies outside from India...
03 April 2014 4,120 1 View
I want some information regarding reference electrodes e.g. SCE or Ag/AgCl of various companies and of which supplier should be in India and cost should be less than Rs.15000.
03 April 2014 4,295 3 View
On which parameters does the thickness of absorbing layer depend?
31 December 2013 1,245 3 View
.
31 December 2013 7,200 5 View
Light trapping.
31 December 2013 4,394 1 View
We use reactive sputtering process to make aluminum nitride film, and want to make c-axis aluminum nitride film on a silicon substrate, but the crystal orientation cannot be seen with...
03 March 2021 7,975 3 View
Hello everyone. Given microstructure image belongs to a 12% ledeburitic cold work tool steel (annealed and tempered). The sample was etched with picral (100 mL ethanol and 4 g picric acid). I...
02 March 2021 4,119 3 View
In some materials, properties such as band gap, thermal conductivity differ along different crystallographic axes. What are the basics?
01 March 2021 1,923 3 View
Hi all, I need to cleave the ester in Ethyl 2-amino-1H-imidazole-5-carboxylate to make the carboxylic acid and retrieve the product from solution to use in downstream applications of linking to...
01 March 2021 8,766 3 View
I try to check the uv-vis absorption of Indium nanoparticle. Now I am measuring in solution, can I measure it in the form of a film?
01 March 2021 930 3 View
Favourable conditions of base pressure, rate of deposition. Also, by which characterisation technique to be used to verify the thickness of the deposited film.
28 February 2021 3,640 3 View
What could be the reason of moisture at the sides of Vial when I am preparing my polmyer+DMSO solution for membrane fabrication? What etiquettes I am possibly missing here?
28 February 2021 6,516 5 View
I am working on modeling and simulation of biomecanical material behaviour, I have succeded on simulating skin using anisotropic hyperelastic material, on APDL and in our lab's finite element...
28 February 2021 552 3 View
Good day to all, I have no experience with light emitting diodes. I am building a glass mini flume to demonstrate the photo degradation of Methylene Blue in water running over self cleaning...
26 February 2021 4,026 5 View
I am working on TiO2 composite material and the results of XRD have a lot of small/junk peaks and while I apply a smooth filter in Origin then the other characteristics peaks disappear so anyone...
26 February 2021 8,183 3 View