Hi, I recently fabricated a flat perovskite (CH3NH3PbI3-xClx and CH3NH3PbI3-xBrx) but unfortunately the Voc is very low (about 0.4V) but the Jsc is considerably high (>20 mA/cm2). I looked...
01 January 1970 7,144 16 View
Do you treat the just TiO2 blocking layer, or both bl-TiO2 and mp-TiO2 when fabricating FTO/bl-TiO2/mp-TiO2/HTM/Au device? I did deposit bl-TiO2, dry at 125 degree C for 5 mins, spincoat meso-TiO2...
01 January 1970 6,413 0 View
Why most of the people used FTO instead of ITO for perovskite solar cell fabrication? I know the band gap of ITO and FTO is 4.9eV and 4.4eV respectively, but is this will make any different?
01 January 1970 8,911 4 View
How to get good and homogeneous layer of compact-TiO2 other than spray pyrolysis or expensive Atomic Layer Deposition in perovskite solar cell fabrication? We want full coverage of this compact...