Hi All, I would like to know about heating rate per min..Is it necessary to apply heating rate 30 to 35 degree per min?will it work to keep heating rate 20 degree per min till 900 degree and...
03 April 2020 8,052 1 View
Hi, I would like to know how to decide parameters especially Gas flow, pressure,temperature for WS2 monolayer growth using CVD technique?I am using WS2 polycrystalline precursor. I appreciate, if...
27 January 2020 9,188 4 View
Hi , I am establishing CVD set up for lateral heterostructure of 2D materials (especially MoS2/WS2) using two zone furnace. I would like to know the parameter need to take care while geting high...
25 January 2020 8,749 0 View
Hi, I would like to grow MoS2 monolayer on Sio2/Si using CVD technique. I would like to the process of substrate cleaning. I appreciate, if some one will suggest me/give feedback for the...
25 January 2020 8,626 8 View
I have done in detail Raman studies for charge transfer between few layer MoS2 and donor and acceptor aromatic molcules (like TCNE, MV etc.).In general FWHM increase with increasing conc. of...