The samples used is 16 mg of CMC-chitosan polymer and reference material (α-Al2O3). The method used was heated from 35 °C to 500 °C at 10 °C min−1 in flowing (50 mL min−1) nitrogen.
I'm agree with these answers. You could have problems with your calibration or the equipment maintenance because the weight change too much to be acceptable.