I am TiO2 thin film using rapid thermal annealing. I have varied the annealing temperature and annealing time as well as ambient. For temperature, peaks are increased but during varying the annealing duration, the intensity peak of XRD increased upto some annealing temperature and after that again decrease in Rapid thermal annealing