I have coated CH3NH3PbCl3 film onto glass substrate via two different methods. First one is one step spin coating method and the other one is electrospinning method. The calculated lattice strain using Williamson and Hall technique (W-H) is higher for Electro-spun film.

What are the possible reason behind such observation?