Dear qll, we fabricated LiNi0.8Co0.15Al0.05O2 by conventiona solid state synthesis and after fabrication of electrode form by using %80/%10/%10 of active material/PVDF/carbon and we are used 1 M LiPF6 (EC/DMC, volume) and (EC:DEC:DMC) and anode electrode is Li metal. we mesured CV in the range of 2-4.5 V but i didnt obtain the graph of expected CV data, does anybody have any suggestions for solving this obstacle ?