Nowadays, the most often utilized procedure is a two-step process that involves lactic acid oligomerization and depolymerization to generate lactide. To generate PLA, however, ring polymerization needs high-purity lactide, which can only be produced with high temperature, vacuum, and energy input during lactide manufacture.