There seems two types of porosity in these SiC bases foams, one "between struts" and the other "in struts". Any idea of the reason of the formation of the second form?
Thanks Hugo
There seems the last one is more probable.
Do you reckon that the SiC based matrix will decompose in around 1300C and lead to these features?
Hi everyone How to model Supercritical water gasification (SCWG) process in Homer software?
25 February 2021 4,075 1 View
Hi every one Is it possible to define biogas as a fuel in the reformer process(scwg) in Homer software? Biogas fuel is not available in the options thanks
23 February 2021 6,518 3 View
I am working on polishing abrasives. I need to do few characterizations ? which can provide the on time surface chemistry of substrate with polishing abrasive during optical polishing. I would...
18 February 2021 5,319 3 View
Hi everyone. I am looking for a high temperature MPCM. More specifically, I need the thermo physical properties of a microencapsulated phase change material with the melting temperature between...
14 February 2021 3,606 2 View
The hourly load curves of the selected household in each season are shown in Fig. 28. Figure 28 shows the demand for electricity in four months on an hourly basis. Can you explain this diagram to...
08 February 2021 657 16 View
Currently using Msc Marc Mentat for FEA. Now i conduct the mesh convergence/sensitivity analysis manually. So I need to know if there any automatic way to conduct the mesh convergence/sensitivity...
04 February 2021 3,310 3 View
Hi, I'm doing molecular dynamics on a 168 atoms system with a 20 A vacuum. To speed up my calculations, I set ALGO = Fast tag in INCAR, but surprisingly VASP crashes momentarily!. I have done a...
25 January 2021 9,876 3 View
Hello everyone, I'm a beginner on the simulation software ANSYS HFSS. I need to know how to measure the size of the generated field of my simulation. I have simulated a geometry that looked like...
20 January 2021 9,113 2 View
I have tried BoltzTrap, and EPW but I'm not sure whether Boltzmann Transport Equation is a right approach for a complex system (semi cond. + an Oxide layer or even the semiconductor itself). Also...
11 January 2021 4,597 4 View
Hello to all What is the gradient thermal annealing (GTA) process?
06 January 2021 7,740 2 View
Question to you and THEM, the New Journal, "Integrative Psychological and Behavioral Science" -- do you not know, and have you not seen, this done before? There appears to be a core problem for...
02 March 2021 3,024 2 View
Hello every body Does any one has any idea to help me choose a reasonable basis set for intermediate metal ions (i.e Fe2+, Mn2+, Cu2+ and exc.) interactions with guanine or other DNA organic...
01 March 2021 6,187 2 View
Im doing PBMC isolation -> CD14+ enrichment using magnetic beads -> stimulation setup. My negative control is just cells in cRPMI but they seem to get activated over and over again.
28 February 2021 7,883 3 View
Is there any reason for decrease in fluorescence emission intensity of HSA,BSA when increase the concentration ?
28 February 2021 3,653 4 View
What could be the reason of moisture at the sides of Vial when I am preparing my polmyer+DMSO solution for membrane fabrication? What etiquettes I am possibly missing here?
28 February 2021 6,516 5 View
The reasoning behind this question is to align the ratios of the proton potential in energy per charge to the speed of light in distance per time. As these two dimensions appear to be related,...
27 February 2021 947 7 View
Its effect appears in real part of ac conductivity also. Can anyone suggest any reason behind it?
26 February 2021 3,487 3 View
I got a thin band and a thick band i guess it would be the genomic DNA and the 260/280 ratio is 3.
21 February 2021 6,523 6 View
Hi Colleagues- What do you think about the following methodological issues: 1. Is it methodologically wrong to formulate quantitative research questionnaire based on inductive reasoning? 2. Is it...
21 February 2021 4,634 6 View
what is the reason film thickness increased when increased doping concentrations give some reasons The measured film thickness is 156, 282, 394, 548 and 681 nm for 0, 1.5, 2.5, 3.5, and 4.5 wt....
17 February 2021 8,987 5 View