17 October 2023 1 7K Report

The Si (1 1 1) was properly cleaned by ultrasonicated and etched prior to fabrication and PEDOT:PSS was also ultrasonicated also. Samples without the above procedure was also tried. 10 mm size samples were used on which PEDOT:PSS was spincoated at different rpm from 1000-3000 rpm. Carbon conductive paste was used for metal contact.