Dear Researchers, I have a problem with the synthesis of the PMMA/PVP blend. I used the chloroform/methanol (90%/10%) as a mixed solvent and the sample annealed at 80C. but after annealing the sample cracks and appears not homogenous!!. Is there any problem with the solvent or with the annealing method?