The TPM treatment ensures the film adheres to the substrate after curing. I use N,N-Methylenebis(acrylamide) as the crosslinker, Darocur as the photoinitiator and DMSO as the solvent. I have tried replicating procedures from a few papers with little luck. I need uniform films less than 1.5 microns thick so I can characterize them with ellipsometry.