1. thermal conductivity - tested at ambient temperature - aged 180 days (C-177)

2. thermal conductivity - tested at -180 deg - fresh foam (C-177)

3. thermal conductivity - tested at -180 deg - aged 180 days (C-177)

4. leachable halide content (ASTM C-871)

5. water absorption at 20 deg C (ASTM D2852)

6. Fire resistive properties (BS-4735):

extent of burn (max.)

extinguishment time (max.)

mean burning rate (max.)

7. Retention of weight (ASTM D-3014)

8. Linear coefficient of thermal exp/contraction (between -165 deg C and +21 deg C) (ASTM D696, BS-4370)

9. Cryogenic thermal stress resistance (CTSR)

a. tensile strength - tested at -165 deg C (ASTM D1623)

b. tensile modulus - tested at -165 deg C (ASTM D1623)

10. friability

11. buttler-chimney for weight retention & extinguish time

12. limited oxygen index

13. maximum smoke density

Regarding test#1 and 3 do we have to wait to get the foam aged 180 days or there is such a machine that can give equal effect to aged 180 days like in coating?