Hi there, I have synthesized selenium nanoparticles coated with different concentrations of chitosan folate polymer, but based on dls and fesem, the size of nanoparticles coated with chitosan folate at higher concentration(0.4w/v versus 0.2w/v) have greater size. Can you explain why?