you can cure under relative humidity (100%) at 40 degree or at 23 degree. the curing is only accelerate the reaction, but at the later ages the strength of both cured at oven and room temperature will be almost same, however the quality of the resulting product is the predominant where the curing at room temperature leads to better rearrangement in the geopolymer structure.