I am currently working with a Ultratech Savannah S100 ALD system. Currently, the system can be pumped down to a base pressure of 80 mTorr. Obviously, there is some room for improvement. But I am...
10 October 2018 8,900 0 View
I understand the importance of a chemically clean, oxide-free surface to produce a high-quality anodizing oxide film. My understanding about electropolishing is that it unavoidably produces a thin...
08 August 2017 7,375 2 View
I am curious about the ion conductivity of the molding compound because it might affect the electrochemical corrosion rate of the electronic materials.
05 May 2017 6,962 3 View
I used to do polarization measurement to obtain corrosion current. Now as I switch to dilute solution, polarization curve needs to be corrected to eliminate the effect of solution resistance,...
02 February 2015 6,087 5 View
Why do we have to make the cathode area and anode area equal when measuring galvanic current using zero resistance ammeter? We can still measure the current density of the cathode and anode by...
08 August 2014 3,845 2 View
What kind of acid should I use for different metals, like Al, Cu and their alloys?
07 July 2014 5,624 4 View