We are finding a hard time to strip of residual HSQ ( Fox 16) after using it as a mask in etching? We are coating 600 nm thick HSQ and writing with 3000 microC/cm^2 dose at 1 nA current. We are...
09 December 2020 5,684 2 View
Hi, Good afternoon. We are trying to make patterns on lithium niobate(which basically glass surface). We are cleaning our chips with acetone and IPA for 5 mins each. To do the pattern, we are...
15 January 2020 9,732 0 View
I am investigating different types of losses in multi junction solar cell. I came to know that, tunneling junction is a important factor for designing multi junction solar cell. What kind of...
14 April 2018 704 3 View