I have prepared graphite oxide from the reaction of graphite,KMnO4,H2SO4 and H3PO4.For reduction of 300 mg of GO I used 600 microlitre hydrazine hydrate and 900 microlitre ammonia...I have got...
05 May 2015 7,250 1 View
I have a 43 degree peak in Xrd of graphite oxide.In some literatures it is written that it is due to the presence of unreacted graphite
02 February 2015 9,619 6 View
I have exfoliated graphite in DI water for couple of hours but by doing this I am getting much higher intensity D' peak than G band
02 February 2015 6,121 4 View
In most papers 95 to 100 degree centigrade is used to synthesize RGO. Why arent temperatures above 100 degree like 150,200,250 used to synthesize graphene?
02 February 2015 9,446 3 View
I am having difficulty to separate unreacted graphite from graphite oxide.
02 February 2015 3,477 5 View
I am trying to synthesize graphene by the following process-Graphite powder (
09 September 2014 6,738 3 View