8 Questions 21 Answers 0 Followers
Questions related from Siva Prasad Murugan
I want to use few images from a published journal and conference proceedings in my manuscript. It is not a review paper. I need those images for preparing the introduction of an original research...
07 July 2018 4,685 5 View
Normally, the hardenability and weldability of advanced high strength steels (AHSS) are expressed in terms of carbon equivalent (CE). I tried to calculate the carbon equivalent of TWIP steel (900...
02 February 2017 9,286 4 View
Dear Researchers, I am working on the dissimilar resistance spot welding of Fe-Mn-C-Al austenitic steel (with other alloying elements such as Si, Ni, Cr, Ti, Mo, Zr, V, Nb etc. in small amount)...
03 March 2016 8,582 11 View
Hello researchers, Can anyone please explain the effects of shrinkage cavity/voids on the mechanical properties of resistance spot welded advanced high strength steels? I could find some journals...
01 January 2016 8,272 5 View
Is there any international codes or standards like API code, AWS code, ASME BPVC which provides the maximum possible number of repair welds that can be done on MS or SS or dissimilar weldments??...
01 January 2015 2,323 5 View
Just imagine we are depositing aluminium over steel using hot dipping or TIG surfacing. Over this specimen can we use PEO technique to fabricate corrosion resistant coating?
12 December 2014 480 15 View
Electrochemical Impedance Spectroscopy is a useful technique to evaluate the corrosion properties of organic and inorganic coatings on metals and alloys. I have used this technique to study the...
12 December 2014 6,811 3 View
I have observed porosity at the HAZ of mild steel side of AISI 304 stainless steel and mild steel dissimilar weld. Welding technique was SMAW and the electrode used was E308L. What may be the...
12 December 2014 9,333 8 View