5 Questions 12 Answers 0 Followers
Questions related from Shiqi Xiao
The Cu foil was first electroplated with a layer of Ni, then the alloy foil was annealed in quartz tube under H2/Ar atmosphere at 1040℃ for 2 hours. But when I open the furnace and cool the tube...
04 April 2016 7,330 5 View
Usually the as grown graphene film is transfered by PMMA, which act as a sacrifice layer. But I found the PMMA residues were very hard to clean thoroughly. Does anyone have another effective...
01 January 2016 9,906 2 View
Methane and hydrogen are used to synthesize large single-crystal graphene. Flow rates of are 0.01sccm and 40sccm respectively. The Cu foil is electropolished to flatten the surface before growth.
12 December 2015 775 6 View
I refered two books, but they gave me the different answers. One said the lower the pressure, the thicker the boundary layer. The other said the oppsite result.
08 August 2015 1,007 2 View
As shown in the attached picture, I found a lot of sphere impurities(100nm) on the surface of the sample. EDS tells the impurities contain Si and O element. Does anyone know how this happens? The...
06 June 2015 2,384 9 View