4 Questions 10 Answers 0 Followers
Questions related from Shashi Kant
Dear all, I am investigating the corrosion resistance of ceramic coating (deposited by PVD process) on Stainless steel samples using Gamry Instrument with parameters OCP (77.78 mV conducting...
20 December 2021 6,351 7 View
Dear all, I am trying to deposit Al over bonding layer on Glass to get Al mirror using RF sputtering. What should be the exact thickness of Al layer to get the stable Al mirror. Also, what should...
27 October 2021 8,607 4 View
hy all, I am trying to deposit Cu on Al, glass using magnetron sputtering at Rt and RF power 250. But the adhesion of the Cu layer to the Al substrate is very low and peeled off using normal...
01 September 2021 8,284 3 View
I am working on ceramic material to check the chemical stability and corrosion resistance, for the seawater/marine environment, what should be the accurate/healthy concentration of the medium...
10 June 2021 3,227 6 View