11 Questions 15 Answers 0 Followers
Questions related from Sajna Ss
Hi, I want to perform Galvanostatic charge/discharge studies using Wonatech SP1 electrochemical workstation. I do not know how to do this. There are two tests showing in this. One is CC/CC test...
07 April 2024 4,230 2 View
I made a nonmaterial with elements Ni, Co, Se, C and O. The compound I attempted is NiCoSe2/GO using required precursors. I tried different literatures and YouTube videos to index the peaks with...
05 September 2023 3,641 0 View
Hi I have performed DPV with one of the material against a pesticides. I found the region just after the oxidation peak was increasing with increasing concentration of pesticides. I am quite...
20 June 2023 9,970 2 View
Hi I have measured the corrosion experiment which is shown below. The experiment shows that the Zre values are going in a negative direction. What is the possible reason for this?. Kindly someone...
12 June 2023 3,131 2 View
I connected the corrosion cell with workstation. The voltage values started fluctuating when connected with corrosion cell before OCP. The values in the voltage relies within in a stable range...
17 April 2023 4,735 8 View
I run an impedance test with mild steel coated with polymer coating. The impedance is showing very abnormal pattern as shown in the pic. On the other hand, when I was running the same Nyquist test...
17 April 2023 9,781 2 View
Hi, I run the OCP corrosion test with the help of corrosion cell keeping Saturate calomel electrode as reference electrode, Stainless steel as working electrode and graphite as the counter...
15 April 2023 5,048 5 View
I run one OCP measurement with corrosion cell using saturated calomel electrode as reference electrode, Metal plate as working electrode, Graphite as counter electrode. As far as my knowledge is...
14 April 2023 7,803 11 View
I prepared a MOF, ZIF through solvothermal method. I run the cyclic voltametry with following conditions. I opted the conditions from the literature. Electrodes : Glassy carbon electrode (WE),...
13 April 2023 807 2 View
I run one CV with Copper sulphide. The slurry composition is as follows. 5 mg material + 850 micro L IPA + 140 microL MilliQ + 5% perfluorinated nafion. I drop cast this on glassy carbon...
12 April 2023 6,555 5 View
Hi I am working on electrochemical sensing applications. The ink (slurry) composition I used in as follows; 5 mg material + 850 microL Isopropanol + 100 micro L Milliq water + 50 microL nafion...
12 April 2023 1,413 0 View