Hello All, In order to make some calcium test devices, we will be needing to expose calcium pads (100 nm of thickness) to nitrogen atmosphere. We do not expect the exposure time to be more than a...
10 September 2019 7,276 4 View
In order to verify the epitaxial nature of the thin films, one can perform a phi scan. The distribution of a certain omega-2theta peak along phi will be indicative of the two-dimensional...
08 May 2014 1,185 2 View
I have GaN and AlN films ranging from 10 nm-150 nm in thickness. For the thicker films, I can use the general theta-2theta coupled scan. But for the thinner films, I have to use the grazing...
23 April 2014 4,821 1 View