3 Questions 6 Answers 0 Followers
Questions related from Pinki ..
I am growing PtTe2 films using direct tellurization of Pt films in CVD system. The Raman spectra of the film is matching well with literature. But the EDAX and XPS results are not coming good. How...
20 March 2023 3,513 3 View
I am depositing thin films of Co using RF sputtering (magnetron) system. The deposition pressure is 7 x 10-3 mbar and RF power is 80 W at 20 sccm Argon flow. Earlier I was getting a sheet...
30 January 2023 1,150 6 View
I tried SnTe2 to exfoliate with scotch tape, but it's not peeling off into layers. How can I exfoliate the materials using another mechanical/chemical method?