I fabricated my perovskite using PEDOT:PSS/MAPbI3/PCBM/Al. After depositing the back contact (Al), I annealed the cell again at 100 degrees for another 10 minutes. I obtained no PCE. I would like...
10 October 2018 5,821 3 View
I deposited both precursor solutions at 2000rpm for 30s and after annealing i got a brown colour.
10 October 2018 9,190 3 View
A dye layer above the perovskite layer