I made Indium Tin Oxide(ITO) thin layer and calculated crystallite size by using Scherrer's formula for XRD results. And I measured film thickness by using alpha step equipment and that value was...
22 August 2016 5,482 6 View
Is Scherrer's formula applicable to use for thin film X-RD results? If anybody knows or if somebody has theoretical details regarding physical relationship between the formula and crystal...
08 August 2016 6,673 5 View
In my ITO sol contains PVA as a binder/stabilizer. I did annealing and I got brown colored layer instead of transparent layer (After annealing my samples were not opaque but it was not good...