5 Questions 5 Answers 0 Followers
Questions related from Muhammad Shoaib
I made several ORR catalyst for PEMFC but after putting the catalyst in vial/glass bottle/polybags, I observe decrease in onset/peak potentials with the passage of time. e.g. if I test my catalyst...
10 March 2019 6,253 1 View
I am doing work on non-precious metal catalyst for ORR. All the times, I get narrow peak using CV while a broader peak using LSV for the same catalyst (as shown in the attached figure) at same...
08 March 2019 7,657 4 View
We have a lab of batteries and fuel cell where we usually work with fuels other than hydrogen like formic acid/ methanol/ NaBH4/etc. A new student has purchased a hydrogen cylinder to use it as...
29 October 2018 7,722 4 View
Do we get the same (or different) onset/half-wave potentials using different templates (like CaCO3,SiO2, or without template) for PEMFC ORR? As far as I know, we get different current densities...
25 June 2018 6,654 2 View
I am new to the field of Fuel cell and working on non-Pt metal catalyst. I want to know how Pt (and some other materials) follow 4 electron transfer while many others (including graphene) follow 2...