5 Questions 10 Answers 0 Followers
Questions related from Mehdi Taherishargh
I applied T6 heat treatment on A356 alloy. Surprisingly, the compression test graphs showed elastic modulus of 97 Gpa which seems odd to me. The yield stress of the alloy calculated to be 276 Mpa...
24 February 2014 6,776 15 View
I am working on a kind of composite material in which expanded perlite particles are as the second phase. There are some references in the same area working on ceramic hollow spheres or...
24 June 2013 7,876 0 View
As a marginal part of my project, I should melt down the PbO along with 8 wt% SiO2 to make a high density glass with low viscosity. But, PbO is so toxic. I wanted to know the best way of mixing...
06 May 2013 3,259 15 View
In our work we need a hot working steel with the service temperature of 1100 Celsius. Actually T300 ma be a good candidate but I am looking for a cheaper one.
12 March 2013 4,884 6 View
We want to do a process in which the NaCl may be entrapped in Aluminum after solidification. I am concerned about the possible corrosion as a result of salt presence in bulk.
20 February 2013 573 11 View