9 Questions 40 Answers 0 Followers
Questions related from Johneph Sukham
What could be the reason for the pin holes on thin film ? The roughness of the film is around 0.40 nm
07 September 2016 4,867 12 View
How to avoid the Glow discharge during sputtering . During deposition the Voltage ramps upto 3 times higher than usual sputtering voltage and there is very less plasma generated and no films were...
05 August 2016 1,345 15 View
Is there any formula to calculate Film thickness from Psi and delta graph as a function of wavelength obtained from Ellipsometry?
23 June 2016 7,417 5 View
What are the ways to remove amino Silane self assembled monolayer chemically which is attached to polymer?
12 April 2016 712 5 View
Has anyone experience with etching or cleaning of Amino silanes using Plasma cleaning ?
12 April 2016 268 6 View
What are the some ways of smoothening a gold film deposited using Sputtering?
08 April 2016 6,950 7 View
What is the role of negative refractive index and negative permittivity of Metamaterials?
07 December 2015 3,235 5 View
Thanks in advance for your replies.
01 April 2015 7,761 2 View
In cst studio suite graphene is not listed as a material . I have read some papers that it can be added as a material too. Please tell me how to add as a material ?