Currently, I have made a good dry mix formula for Geopolymer from Fly ash and slag. We are ready for scaling up the production to help to solve the problem of fly ash in our country. What I have...
06 August 2017 7,603 2 View
Dear All, as we have to cast the Geopolymer concrete insitu at sea island, if sea water to be used can we add 5% OPC to accelerate curing in ambient temperature. The fly ash with 1.5% CaO and we...
29 July 2016 8,274 3 View
we do have efflorescence problem with our GPC concrete after demolding 4-5 days as air moisture content is high to leach the salt probably Na2CO3. They looked like the needle crystals. How can we...
08 July 2016 3,690 4 View
Since handling/transport of the alkaline solution to site very difficult and dangerous we would like to premix Fly ash with Sodium Hydroxide(lye), sodium silicate powder in one package in a...
29 May 2016 2,802 6 View
I want to increase the setting of Geopolymer concrete by adding small quantity of CaSO4 In to the mix and by doing that I can reduce the shrinkage and minor cracks especially in making Geopolymer...
02 May 2016 5,595 1 View
Can we add up spent FCC catalysts into the fly ash based geopolymer? How many percent wt is good enough?