4 Questions 4 Answers 0 Followers
Questions related from Hesamoddin Rabiee
hi i want to use sodium borohydride (NaBH4) as the agent for reducing metal ions on CNT and obtain metal-coated CNTs. i have a few questions: 1. if my solvent is ethylene glycol, can i use the...
16 April 2021 9,617 1 View
hi all, i am trying to electrodeposit Sn on Cu, and some carbon substrate. my electrolyte is SnCl2.2H2O in a 2M KOH solution. i notice that after adding SnCl2.2H2O to KOH solution a very...
24 August 2019 977 3 View
hi all, i have an Agilnet GC 7890a TCD. i was wondering how much sample injection is needed for the TCD detector to get a decent peak? for example, i dont get a good peak when i inject 5...
04 June 2019 2,507 11 View
Hi, Does anyone know where to buy composite hollow fiber membranes/modules with a thin layer of PDMS?? most of the suppliers have thick PDMS membranes with thickness from 50 to 100 micrometer....
14 May 2018 8,765 2 View