I want to make electrospinning scaffold with PLA/PCL/PMMA/Collagen with these methods: 1. I use chloroform:methanol 3:1 to dissolve PLA (mW 80.000, 2 wt%), PCL (mW 70.000, 3 wt%), and PMMA mW...
02 November 2019 6,181 5 View
For my thesis research, I dissolved PLA and PCL in chloroform: methanol (3:1), PMMA (350.000 MW, 13 wt%) in acetone, and collagen in acetate acid--and then, I mixed them together. The problem is...
07 October 2019 8,405 4 View
For my thesis research, first, I mix PLA (solvent: chloroform/methanol) and PCL (solvent: chloroform/methanol) for 2-3 hours. After that, I want to mix PLA/PCL with PMMA (mW 350.000 solvent: ethyl...
03 October 2019 7,273 1 View
Greetings! I have a research where I dissolve PLA in chloroform:methanol (3:1) for 3 hours and also PCL in chloroform:methanol (3:1) for 3 hours too. After that, I have to blend those two polimers...
18 September 2019 3,493 3 View
Greetings! I have a research about electrospun membrane synthesis where I dissolve PLA pellets in chloroform:methanol (3:1) for 3 hours and also PCL pellets in chloroform:methanol (3:1) for 3...
18 September 2019 5,320 2 View
Greetings! I have made an electrospun membrane with PLA (~ 65.000 mW) maximum transmittance of spectra 60 %, PCL (80.000 mW) maximum transmittance of spectra 90%, PMMA (350.000 mW) with maximum...