3 Questions 4 Answers 0 Followers
Questions related from Eisha Khalid
I have tested FeMn-based porous materials in SBF (immersion). Now it is required to clean the corrosion products for further testing. Conventionally, a solution of HCl and Hexamethylene Tetramine...
09 February 2025 2,012 2 View
I am using Weck's Reagent (4% KMnO4, 1% NaOH in distilled water) to etch 6061. But at higher magnification, the grains are not showing at all. The chemicals are up-to-date and are not expired....
30 June 2021 4,918 10 View
I am using a Tungsten-based tool to friction stir weld aluminum sheets. The material sticks to the tool after welding and it is difficult to get rid of it. Can anyone suggest cleaning strategies...
14 June 2021 7,904 3 View