5 Questions 4 Answers 0 Followers
Questions related from Boudnani Zeine Elabidine
As highly modified rubberized binders tend to be flexible than stiffer by showing less stiffness and higher deflections in BBR test, that means higher ability to resist cracking at low temperature.
06 March 2020 1,828 0 View
For experts, specialists, researchers, academic and students: Why the rubberised mixes show higher cracking resistance by showing higher fracture energy as rubber content increases?. In other...
10 February 2020 328 0 View
Numerical methods, experimental Methods...etc
27 December 2018 5,627 2 View
The absence of shearing mixing specifications for asphalt rubber is still a black point in the agencies specifications despite its high effect on the viscosity of the final asphalt rubber so there...
16 October 2018 8,036 1 View
Just i want to see how much the science treats the use of tires waste in highways construction at all levels.
12 February 2018 8,348 2 View