Hi everyone, i've etched a PM mark on a 5.1kA Oxide layer and i've been getting lower mark signal strength (~5-10%). I've been using ma-N 1410 PR type (1um), i noticed discoloration on the marker,...
02 October 2018 9,793 1 View
Suffered Silver peeling on ITO (indium tin Oxide), using HMDS for adhesion. Is contact angle check a good guage to check the adhesiveness? Silver is hydrophilic? and if my surface condition of...