I am synthesizing Graphene Oxide from Anthracite Coal. Anthracite coal was first pre-treated with 30% HNO3 for 2 hours at 80 oC temperature. Then washed with distilled water several times until...
29 October 2020 8,196 1 View
I am working on anthracite coal and trying to change its amorphous structure. After deashing and devolatilization, what other possible ways are there to induce stacked or layered structure in it...