4 Questions 1 Answers 0 Followers
Questions related from Aynur Inan
Which atmosphere can I sinter Ti64 green bodies without oxidizing? I use 5% H2, balanced argon atmosphere but my samples still oxidize at 1250'C.
04 August 2024 2,606 0 View
I will use polyurethane foam for replica impregnation method. I want to increase hydrophilicity of polyurethane. Which chemical should I treat the surface of the polyurethane foam to increase its...
11 March 2024 7,827 2 View
I want to produce Ti64 trabeculer structure by replica impregnation method but during sintering my foams collapse. I tried multiple coating but during impregnation first coating moved away form...
25 September 2023 6,142 0 View
How can I increase strength of metallic foam produced by replica impregnation method? I am trying to produce the Ti64alloys metallic foam by replica impregnation method. But after sintering I...
23 September 2022 1,215 0 View