I have taken 300mg of MWCNT, heated it for 3 hours under reflux in 100 ml of mixture acid (H2SO4 + HNO3) in a 3:1 ratio, and maintained the temperature at 95 degrees. I am using a PTFE membrane...
02 February 2014 6,648 9 View
Concentration used during functionalization was: sulfuric acid - 98wt% and nitric acid - 69-72 wt%.
01 January 2014 7,831 2 View