Does anyone has previously worked on micro-structural analysis of mild steel electric arc welded, heat treated joints...
01 January 2019 9,853 2 View
I have heat treated mild steel welded joints using E6013 electrode from 600 to 900 degree centigrade at 100 degree temperature difference. Specimens were then cooled in air. What could be the...
01 January 2019 9,253 0 View
Hi Everyone. i have some confusion. i am currently working on crack growth study in mild steel using Paris Law. But the problem is how to find the constants?. Second i am applying fatigue load as...
03 March 2017 766 3 View
In Fatigue Crack growth study We should keep stress ratio always positive or we can keep it negative as well (stress ratio (R)= Min Stress/Max Stress). Note: Specimen is compact tension one,...