Use any non-ionic surfactant, for example, a polyoxyethylene alkyl ether.Do not use anionic surfactant, since a precipitate with your cationic polyelectrolyte will precipitate.Aluminum salts as a result of hydrolysis form water-soluble hydroxides, the particles of which acquire a positive charge. Therefore, they will be combined with your cationic polyelectrolyte.